Relative Density @ 60/60 °F
Method ASTM : D-1298
SPECIFICATION : Reported
Flash Point P.M.C.C.
UNIT : °C
Method ASTM : D-93
SPECIFICATION : min. 55
Kin. vis. @ 40 °C
UNIT : cSt
Method ASTM : D-445
SPECIFICATION : 1.60-7.00
Redwood Viscosity 1 @ 40 °C
UNIT : Sec
Method ASTM : IP-70
SPECIFICATION :30-43
Color ASTM
Method ASTM : D-1500
SPECIFICATION : max 4
Sulphur ,Total
UNIT :% mass
Method ASTM : D-4294
SPECIFICATION : max 1.00
Pour Point
UNIT : °C
Method ASTM : D-97
SPECIFICATION : max +3 – max +9 – max +15
Water and Sediment
UNIT :% (Vol.)
Method ASTM : D-2709
SPECIFICATION : max. 0.10

Heat of combustion
UNIT :MJ/Kg
Method ASTM : D-4868
SPECIFICATION : 44.3
Ash Content
UNIT :% mass
Method ASTM : D-482
SPECIFICATION : max.0.01
Corrosion Copper Strip (3 hrs @ 100 °C)
UNIT : rating
Method ASTM : D-130
SPECIFICATION : max. 1
Carbon Residue
UNIT : % mass
Method ASTM :D-4530
SPECIFICATION : max.0.10
Recovered @ 350 °C
UNIT : %
SPECIFICATION : min. 85
Inorganic Acid ity and Bases
UNIT : mgKOH/gm
Method ASTM : IP-182
SPECIFICATION : NIL